Flame-Retardant Antistatic ABS DGK-ABS KJD789FA

V-0 antistatic ABS for instrument and equipment housings

DGK-ABS KJD789FA is a flame-retardant, antistatic ABS for electronic housings and electrical assemblies. It carries a UL 94 V-0 result with 10⁷–10⁹ surface resistance, 36 MPa flexural strength and a 32 g/10 min melt flow rate that fills thin instrument housings in natural pellets at 1.26 g/cm³.

Instrument housings, equipment covers, internal supports and electrical assemblies are the target parts. A 75 °C Vicat softening temperature (GB/T 1633-2000) suits indoor electronic duty, 7.4 kJ/m² Charpy notched and 29 kJ/m² unnotched impact strength cover assembly knocks, and 13% elongation at break keeps snap features flexible.

Important parameters

Base resin
ABS
Model
DGK-ABS KJD789FA
Color
Natural
Processing
Injection molding
Key performance
Flame-retardant, antistatic ABS with surface resistance of 10⁷–10⁹ and a V-0 result.
Status
Pellets

FAQ

What is this grade made of?

It is a flame-retardant, antistatic ABS with a UL 94 V-0 result and 10⁷–10⁹ surface resistance, supplied as natural pellets. Flexural strength is 36 MPa, tensile strength 21.8 MPa and density 1.26 g/cm³, giving housings a rigid shell with static control for sensitive electronics.

What parts can use this grade?

Natural-color pellets suit instrument housings, equipment covers, internal supports and electrical assemblies. The 32 g/10 min melt flow rate fills thin walls and fine ribs, while 1620 MPa flexural modulus and 29 kJ/m² Charpy unnotched impact strength handle covers that take handling loads.

How is it processed?

It is processed by injection molding, with 85 °C drying for 4–5 hours, 195–210 °C injection temperature and a 70 °C mold in the reference settings. Melt flow rate is 32 g/10 min and density 1.26 g/cm³, so thin instrument housings and internal supports fill at moderate pressure.

How can I request a trial sample?

Share the part drawing, wall thickness and electrical requirements when requesting a sample, and DEYU will match a DGK-ABS KJD789FA grade for trial molding. State the target resistance within 10⁷–10⁹ and the flammability thickness, so the sample specification lines up with your housing design.

Application areas

Application areaTypical parts
ElectronicsInstrument housings
Industrial equipmentEquipment covers
Electrical assembliesInternal supports

Reference quote

Minimum price
USD 8.00/kg
Maximum price
USD 8.50/kg

Final pricing depends on color, order quantity and project requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NameABSGradeDGK-ABS KJD789FA
Material propertiesFlame-retardant, antistatic ABS with surface resistance of 10⁷–10⁹ and a V-0 result.ColorNatural
Specimen dimensions80 × 10 × 4 mmSample formPellets
Processing methodInjection molding——
PropertyConditionTest methodValueUnit
Mechanical properties
Flexural strength—GB/T 9341-200836MPa
Flexural modulus—GB/T 9341-20081620MPa
Tensile strength20 mm/minGB/T 1040-200621.8MPa
Yield strength—GB/T 1040-200620.7MPa
Elongation at break—GB/T 1040-200613%
Charpy notched impact strength—GB/T 1043.1-20087.4kJ/m²
Charpy unnotched impact strength—GB/T 1043.1-200829kJ/m²
Izod notched impact strength—GB/T 1843-20008.5kJ/m²
Other properties
Melt flow rate—GB/T 3682-200032g/10 min
Density—GB/T 1033-19861.26g/cm³
Vicat softening temperature (see note)A120GB/T 1633-200075°C
Surface resistance—GB/T 1401-200210⁷–10⁹Ω·cm
FlammabilityUL 94GB/T 2408-1996V-0—
Injection molding conditions
Drying temperature85 °CDrying time4–5 h
Injection temperature195–210 °CMold temperature70 °C

Surface resistance 10⁷–10⁹ Ω·cm to GB/T 1401-2002; UL 94 V-0; 32 g/10 min melt flow and 1.26 g/cm³ density.

Contact

Focused on modified plastic R&D and production

We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.