Light-Shielding ABS Pellets DGK-ABS ZG176A
Opaque ABS grade for light-blocking housings and LED-adjacent molded parts
Opaque light-shielding ABS; a 2 mm housing wall can block light when placed close to LED beads.
Light-shielding ABS compound DGK-ABS ZG176A for opaque housings, LED-adjacent parts, electronic accessories, light-blocking covers, instrument parts and molded components where a 2 mm wall must block light. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- ABS
- Model
- DGK-ABS ZG176A
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Opaque light-shielding ABS; a 2 mm housing wall can block light when placed close to LED beads.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can the key performance be customized?
Yes. DEYU can adjust strength, flow, color, filler system and special properties according to the part drawing and test conditions.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-ABS ZG176A or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | LED diffusers |
| Application area 2 | sensor shading shells |
| Application area 3 | display frames |
| Application area 4 | white light-blocking covers |
| Application area 5 | indicator lamp covers |
| Application area 6 | optical appliance parts |
Reference quote
- Minimum price
- USD 5.9/kg
- Maximum price
- USD 10.8/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | ABS composite | Specification | DGK-ABS ZG176A |
|---|---|---|---|
| Material properties | Opaque, light-shielding | Color | White |
| Use | Electronic and electrical accessories | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Others | ||||
| Density | 23℃ | ASTM D-792 | 1.1 | g/cm3 |
| Water absorption | 23℃ / 24 h | ASTM D-570 | 0.3 | % |
| Melt Flow Index | 220℃ / 10 kg | ASTM D-1238 | 23 | g/10 min |
| Mechanical Properties | ||||
| Elongation at break | 50 mm/min | ASTM D-638 | 15 | % |
| Izod notched impact strength | 1/4 in. notched | ASTM D-256 | 100 | kg-cm/cm |
| Rockwell hardness | / | ASTM D-785 | 16 | R |
| Bending strength | 5 mm/min | ASTM D-790 | 600 | kg/cm2 |
| Tensile strength | 50 mm/min | ASTM D-638 | 400 | kg/cm2 |
| Thermal Properties | ||||
| Vicat softening point | 5 kg, 50℃/h | ASTM D-1525 | 103 | ℃ |
| Heat distortion temperature | 18.6 kg/cm2 | ASTM D-259 | 93 | ℃ |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1