Light-Shielding AES Pellets DGK-AES ZG8100
Titanium white light-shielding AES for opaque covers and molded appearance parts
Opaque light-shielding AES compound in titanium white, with custom color matching support for molded appearance parts.
Light-shielding AES compound DGK-AES ZG8100 in titanium white for opaque covers, LED-adjacent housings, appliance shells, electronic parts, color-matched appearance components and outdoor molded products. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- AES
- Model
- DGK-AES ZG8100
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Opaque light-shielding AES compound in titanium white, with custom color matching support for molded appearance parts.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can the key performance be customized?
Yes. DEYU can adjust strength, flow, color, filler system and special properties according to the part drawing and test conditions.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-AES ZG8100 or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | LED diffusers |
| Application area 2 | sensor shading shells |
| Application area 3 | display frames |
| Application area 4 | white light-blocking covers |
| Application area 5 | indicator lamp covers |
| Application area 6 | optical appliance parts |
Reference quote
- Minimum price
- USD 5.9/kg
- Maximum price
- USD 10.8/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Technical data
Engineering Data Availability Table
| Name | Light-Shielding AES Pellets DGK-AES ZG8100 | Specification | DGK-AES ZG8100 |
|---|---|---|---|
| Material properties | Opaque light-shielding AES compound in titanium white, with custom color matching support for molded appearance parts. | Color | Custom color matching supported |
| Sample state | Pellet compound | Processing method | Injection molding. Injection molding, extrusion or other processes according to the formula. |
| Data status | Engineering confirmation required | - | Contact a DEYU engineer |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Optical Properties | ||||
| Light shielding rate | / | / | Contact a DEYU engineer | / |
| Light transmittance | / | / | Contact a DEYU engineer | / |
| Color difference | / | / | Contact a DEYU engineer | / |
| Mechanical Properties | ||||
| Tensile strength | / | / | Contact a DEYU engineer | / |
| Bending strength | / | / | Contact a DEYU engineer | / |
| Flexural modulus | / | / | Contact a DEYU engineer | / |
| Izod notched impact strength | / | / | Contact a DEYU engineer | / |
| Weathering Properties | ||||
| UV resistance | / | / | Contact a DEYU engineer | / |
| Weather resistance | / | / | Contact a DEYU engineer | / |
| Thermal Properties | ||||
| Heat distortion temperature | / | / | Contact a DEYU engineer | / |
| Vicat softening point | / | / | Contact a DEYU engineer | / |
| Processing Recommendations | ||||
| Drying temperature | Contact a DEYU engineer | Drying time | Contact a DEYU engineer | |
| Injection temperature | Contact a DEYU engineer | Mold temperature | Contact a DEYU engineer | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1