MoS2 Wear-Resistant PA6 Pellets DGK-PA6 G25MS

PA6 with MoS2 for wear-resistant, low-friction sliding components

MoS2 reinforced PA6; high wear resistance and self-lubricating performance for sliding and rotating parts.

MoS2 filled wear-resistant PA6 compound DGK-PA6 G25MS for bushings, gears, sliding parts, automotive components, mechanical supports and low-friction molded parts requiring durability under movement. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
PA6
Model
DGK-PA6 G25MS
Color
Custom color matching supported
Processing
Injection molding. Injection molding, extrusion or other processes according to the formula.
Key performance
MoS2 reinforced PA6; high wear resistance and self-lubricating performance for sliding and rotating parts.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can wear resistance and friction be customized?

Yes. PTFE, MoS2, aramid or other wear additives can be adjusted according to the mating material, load and movement speed.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-PA6 G25MS or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1chair castors
Application area 2gears
Application area 3guide sliders
Application area 4bushings
Application area 5rollers
Application area 6textile machine sliding parts

Reference quote

Minimum price
USD 5.9/kg
Maximum price
USD 10.8/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePA6/MoS2 compositeSpecificationDGK-PA6 G25MS
Material propertiesHigh wear resistance, self-lubricatingColorGray
UseAutomotive parts, bushings, gear parts, etc.Sample statePellets
Processing methodInjection molding-/
ItemConditionMethodDataUnit
Mechanical Properties
Bending strength2 mm/minGB/T 9341-2008138MPa
Flexural modulus2 mm/minGB/T 9341-20085534.1MPa
Tensile strength50 mm/minGB/T 1040-2006130.8MPa
Tensile modulus50 mm/minGB/T 1040-20061564.3MPa
Elongation at break50 mm/minGB/T 1040-20066.69%
Charpy notched impact strength23℃GB/T 1043.1-20088.4kJ/m2
Charpy unnotched impact strength23℃GB/T 1043.1-200824.9kJ/m2
Cantilever beam unnotched impact strength23℃GB/T 1843-200040.4kJ/m2
Cantilever beam notched impact strength23℃GB/T 1843-200010.1kJ/m2
Others
Melt Flow Index255℃ / 5 kgGB/T 3682-20008.8g/10 min
Density/GB/T 1033-19861.3g/cm3
Heat distortion temperature0.45 MPaGB/T 1634-2000145℃
Surface resistivity/GB/T 1401-200210^8ohm/sq
FlammabilityUL-94GB/T 2408-1996HB/
Injection molding process
Drying temperature120℃Drying time4-5 h
Injection temperature250-260℃Mold temperature90℃

Contact

Focused on modified plastic R&D and production

We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.