Graphite-Filled Wear-Resistant Antistatic PA6 DGK-PA6 PA16SM

Self-lubricating graphite PA6 for gears and bushings

DGK-PA6 PA16SM is a graphite-filled PA6 that combines wear resistance, self-lubrication and antistatic functionality in dark gray pellets. Flexural strength of 89.4 MPa and tensile modulus of 879.5 MPa give gears and bushings the stiffness to carry load without external lubrication.

Gears, self-lubricating bushings and sliding structural parts are the typical applications. A 134 °C heat deflection temperature at 0.45 MPa (GB/T 1634) and 2629 MPa flexural modulus let motion components hold tolerance in warm running conditions, while 14.7% elongation at break gives gear teeth and sleeves room to absorb impact.

Important parameters

Base resin
PA6
Model
DGK-PA6 PA16SM
Color
Dark gray
Processing
Injection molding
Key performance
Graphite-filled PA6 combining wear resistance, self-lubrication and antistatic functionality.
Status
Pellets

FAQ

What is this grade designed for?

It is a graphite-filled PA6 for injection-molded parts that need wear resistance, self-lubrication and antistatic functionality. Flexural strength is 89.4 MPa, tensile strength 59 MPa and Charpy unnotched impact strength 42 kJ/m², so gears and bushings carry load while the graphite keeps sliding contact smooth.

What is its surface resistance?

The grade is supplied as an antistatic, graphite-filled compound for gears, bushings and sliding parts. Resistance level tracks part geometry and graphite dispersion, so DEYU matches it to your target range when the sample is prepared. State the resistance you need with the drawing and the sample grade is selected against it.

Which parts can use this grade?

Typical parts are gears, self-lubricating bushings and sliding structural parts such as guides and supports. Use the mechanical base of 89.4 MPa flexural strength, 2629 MPa flexural modulus and 134 °C heat deflection temperature at 0.45 MPa to size the part; wear then follows the mating material, load and speed of your assembly.

Can I request a molding trial sample?

Share the part drawing, mating material, load and antistatic requirements and DEYU will match a DGK-PA6 PA16SM sample for a molding trial. Dark gray pellets run at 7.92 g/10 min melt flow rate (230 °C / 2.16 kg) in standard injection molding, and the 134 °C heat deflection temperature covers warm duty.

Application areas

Application areaTypical parts
Motion componentsGears and self-lubricating bushings
Structural componentsSliding guides and support parts

Reference quote

Minimum price
USD 4.00/kg
Maximum price
USD 4.50/kg

Final pricing depends on order quantity and project requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePA6 compoundGradeDGK-PA6 PA16SM
Material propertiesGraphite-filled, wear-resistant, self-lubricating and antistaticColorDark gray
ApplicationGears, self-lubricating bushings and structural componentsSample formPellets
Processing methodInjection molding——
PropertyConditionTest methodValueUnit
Mechanical properties
Tensile strength50 mm/minGB/T 104059MPa
Elongation at break50 mm/minGB/T 104014.7%
Tensile modulus50 mm/minGB/T 1040879.5MPa
Flexural strength2 mm/minGB/T 934189.4MPa
Flexural modulus2 mm/minGB/T 93412629MPa
Izod notched impact strength23 °CGB/T 18438.1kJ/m²
Charpy notched impact strength23 °CGB/T 10435kJ/m²
Charpy unnotched impact strength23 °CGB/T 104342kJ/m²
Other properties
Density—GB/T 10331.23kg/m³ †
Melt flow rate230 °C / 2.16 kgGB/T 36827.92g/10 min
Heat deflection temperature0.45 MPaGB/T 1634134°C
Flammability—UL 94HB—

Mechanical values from the DGK-PA16SM-A report; 1.23 g/cm³ density and 7.92 g/10 min melt flow at 230 °C / 2.16 kg.