Carbon Fiber Reinforced PA66 Pellets DGK-PA66 CF15L-CF40L
Custom 15%-40% carbon fiber PA66 for high-strength structural molding
Customizable 15%-40% carbon fiber reinforced PA66; high strength, high stiffness and conductive performance.
Carbon fiber reinforced PA66 compound DGK-PA66 CF15L-CF40L with customizable 15%-40% fiber content for high-strength mechanical parts, electronic components, brackets, housings, fixtures and structural molded products. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- PA66
- Model
- DGK-PA66 CF15L-CF40L
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Customizable 15%-40% carbon fiber reinforced PA66; high strength, high stiffness and conductive performance.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can stiffness and carbon fiber content be customized?
Yes. Fiber level, flow and shrinkage can be tuned around stiffness, part size and surface requirements.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-PA66 CF15L-CF40L or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | lightweight brackets |
| Application area 2 | structural housings |
| Application area 3 | robot arm covers |
| Application area 4 | battery component holders |
| Application area 5 | precision frames |
| Application area 6 | metal-replacement supports |
Reference quote
- Minimum price
- USD 3.5/kg
- Maximum price
- USD 12.5/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | PA66 carbon fiber composite | Specification | DGK-PA66 CF30L |
|---|---|---|---|
| Material properties | High strength, high stiffness, conductive | Color | Black |
| Use | Mechanical parts, electronic and electrical equipment | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | 2 mm/min | GB/T 9341-2008 | 257.5 | MPa |
| Flexural modulus | 2 mm/min | GB/T 9341-2008 | 15536.5 | MPa |
| Tensile strength | 50 mm/min | GB/T 1040-2006 | 186.5 | MPa |
| Tensile modulus | 50 mm/min | GB/T 1040-2006 | 2636.5 | MPa |
| Elongation at break | 50 mm/min | GB/T 1040-2006 | 7.5 | % |
| Charpy notched impact strength | 23℃ | GB/T 1043.1-2008 | 4.4 | kJ/m2 |
| Charpy unnotched impact strength | 23℃ | GB/T 1043.1-2008 | 19.6 | kJ/m2 |
| Cantilever beam unnotched impact strength | 23℃ | GB/T 1843-2000 | 50.2 | kJ/m2 |
| Cantilever beam notched impact strength | 23℃ | GB/T 1843-2000 | 13.3 | kJ/m2 |
| Others | ||||
| Melt Flow Index | 285℃ / 5 kg | GB/T 3682-2000 | 63.6 | g/10 min |
| Density | / | GB/T 1033-1986 | 1.288 | g/cm3 |
| Heat distortion temperature | 1.8 MPa | GB/T 1634-2000 | 225 | ℃ |
| Surface resistance | 23℃ | GB/T 1401-2002 | 10^3-10^4 | ohm-cm |
| Flammability | UL-94 | GB/T 2408-1996 | HB | / |
| Injection molding process | ||||
| Drying temperature | 130℃ | Drying time | 3-4 h | |
| Injection temperature | 275-285℃ | Mold temperature | 90℃ | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1