PC/ABS Alloy Pellets DGK-PC/ABS T85

PC/ABS alloy with dimensional stability for housings and appearance parts

PC/ABS alloy with good dimensional accuracy, easy processing, high rigidity and a high-gloss DEYU finish.

PC/ABS alloy compound DGK-PC/ABS T85 with dimensional stability and easy processing for automotive interiors, electronic housings, appliance shells, printer parts, control panels and molded appearance components. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
PC/ABS
Model
DGK-PC/ABS T85
Color
Custom color matching supported
Processing
Injection molding. Injection molding, extrusion or other processes according to the formula.
Key performance
PC/ABS alloy with good dimensional accuracy, easy processing, high rigidity and a high-gloss DEYU finish.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can the key performance be customized?

Yes. DEYU can adjust strength, flow, color, filler system and special properties according to the part drawing and test conditions.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-PC/ABS T85 or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1custom molded housings
Application area 2industrial fittings
Application area 3appliance parts
Application area 4technical clips
Application area 5functional plastic components
Application area 6extruded or molded profiles

Reference quote

Minimum price
USD 5.9/kg
Maximum price
USD 10.8/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePC/ABS compositeSpecificationDGK-T85
Material propertiesExcellent mechanical properties, dimensional stabilityColorBlack
UseElectronic appliances, automotive partsSample statePellets
Processing methodInjection molding-/
ItemConditionMethodDataUnit
Mechanical Properties
Bending strength2 mm/minASTM D79090MPa
Flexural modulus2 mm/minASTM D7902400MPa
Tensile strength50 mm/minASTM D63858MPa
Tensile modulus1 mm/minASTM D63824000MPa
Yield strength50 mm/minASTM D63847MPa
Elongation at break50 mm/minASTM D63850%
Notched impact strength of cantilever beam23℃ASTM D256650J/m
Others
Density23℃ASTM D7921130kg/m3
Shrinkage rate2 mmASTM D9550.5-0.7%
Melt Flow Index260℃ / 5 kgASTM D123819g/10 min
Heat distortion temperature1.82 MPa, 120℃/hASTM D648105℃
Vicat softening point50 N, 120℃/hASTM D1525125℃
FlammabilityUL-94/HB/
Injection molding process
Drying temperature/Drying time/
Injection temperature/Mold temperature/

Contact