Light Diffusion PC Pellets DGK-PC F295AA

Light diffusion PC for uniform LED covers, panels and lighting components

Light diffusion PC; balanced transmittance and haze for uniform light output and low glare.

Light diffusion PC compound DGK-PC F295AA with balanced transmittance for LED covers, diffuser panels, light boxes, lamp shades, optical housings and molded lighting components requiring uniform light output. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
PC
Model
DGK-PC F295AA
Color
Custom color matching supported
Processing
Injection molding / extrusion. Injection molding, extrusion or other processes according to the formula.
Key performance
Light diffusion PC; balanced transmittance and haze for uniform light output and low glare.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can the key performance be customized?

Yes. DEYU can adjust strength, flow, color, filler system and special properties according to the part drawing and test conditions.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-PC F295AA or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1LED diffusers
Application area 2sensor shading shells
Application area 3display frames
Application area 4white light-blocking covers
Application area 5indicator lamp covers
Application area 6optical appliance parts

Reference quote

Minimum price
USD 5.9/kg
Maximum price
USD 10.8/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Technical data

Engineering Data Availability Table

NameLight Diffusion PC Pellets DGK-PC F295AASpecificationDGK-PC F295AA
Material propertiesLight diffusion PC; balanced transmittance and haze for uniform light output and low glare.ColorCustom color matching supported
Sample statePellet compoundProcessing methodInjection molding / extrusion. Injection molding, extrusion or other processes according to the formula.
Data statusEngineering confirmation required-Contact a DEYU engineer
ItemConditionMethodDataUnit
Optical Properties
Light transmittance//Contact a DEYU engineer/
Haze//Contact a DEYU engineer/
Light diffusion uniformity//Contact a DEYU engineer/
Basic Properties
Melt Flow Index//Contact a DEYU engineer/
Density//Contact a DEYU engineer/
Mechanical Properties
Tensile strength//Contact a DEYU engineer/
Bending strength//Contact a DEYU engineer/
Flexural modulus//Contact a DEYU engineer/
Izod notched impact strength//Contact a DEYU engineer/
Thermal Properties
Heat distortion temperature//Contact a DEYU engineer/
Vicat softening point//Contact a DEYU engineer/
Flammability//Contact a DEYU engineer/
Processing Recommendations
Drying temperatureContact a DEYU engineerDrying timeContact a DEYU engineer
Injection temperatureContact a DEYU engineerMold temperatureContact a DEYU engineer

Contact

Focused on modified plastic R&D and production

We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.