Wear-Resistant PC/PTFE DGK-PC TF1100N

Self-lubricating PC/PTFE for sliding guides and bushings

DGK-PC TF1100N is a PC/PTFE compound built for wear resistance and internal lubrication. Flexural strength of 912 kg/cm² with 110% elongation at break gives sliding guides and bushings a tough, compliant surface, and 1.2 g/cm³ density keeps moving parts light.

Sliding guides and bushings, guide blocks and support parts, and wear strips in equipment all suit this grade. Heat deflection temperature is 118 °C at 0.46 MPa (ASTM D648), and the 13.8 g/10 min melt flow rate fills thin guide sections; the compound is supplied as natural pellets for injection molding.

Important parameters

Base resin
PC
Model
DGK-PC TF1100N
Color
Natural
Processing
Injection molding
Key performance
A PC/PTFE compound designed for wear resistance and internal lubrication.
Status
Pellets

FAQ

What is this grade made of?

It is a PC/PTFE compound designed for wear resistance and internal lubrication, supplied as natural pellets. Polycarbonate provides 912 kg/cm² flexural strength and 110% elongation at break while PTFE supplies the low-friction surface. Density is 1.2 g/cm³, heat deflection temperature 118 °C at 0.46 MPa and flammability V-2 at 1.5 mm.

What parts can use this grade?

Natural-color pellets suit sliding guides, bushings and moving parts with repeated contact. Flexural modulus is 22800 kg/cm² and notched Izod impact strength 78 kg·cm/cm, giving stiffness with impact tolerance for guide blocks and wear strips. Wear performance follows the mating material, load and sliding speed of the assembly.

How is it processed?

It is supplied as pellets for injection molding, with 110 °C drying for 4–5 hours, 255–275 °C injection temperature and an 80 °C mold in the reference settings. Melt flow rate is 13.8 g/10 min and density 1.2 g/cm³, so thin guide sections and bushing walls fill readily.

How can I request a trial sample?

Share the part drawing, mating material, load and sliding speed and DEYU will match a DGK-PC TF1100N sample for a molding trial. Include the wear surface geometry and the target part life, so the PTFE-loaded compound is matched to the contact pressure and speed of the application.

Application areas

Application areaTypical parts
Motion componentsSliding guides and bushings
Industrial assembliesGuide blocks and support parts
Equipment partsWear strips and sliding supports

Reference quote

Minimum price
USD 6.50/kg
Maximum price
USD 7.10/kg

Final pricing depends on color, order quantity and project requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePC/PTFEGradeDGK-PC TF1100N
Material propertiesA PC/PTFE compound designed for wear resistance and internal lubrication.ColorNatural
Specimen dimensions80 × 10 × 4 mmSample formPellets
Processing methodInjection molding——
PropertyConditionTest methodValueUnit
Mechanical properties
Flexural strength—ASTM D790912kg/cm²
Flexural modulus—ASTM D79022800kg/cm²
Tensile strength—ASTM D638630kg/cm²
Elongation at break—ASTM D638110%
Charpy notched impact strength—ASTM D256 †62kg·cm/cm
Izod notched impact strength—ASTM D25678kg·cm/cm
Other properties
Melt flow rate—ASTM D1228 †13.8g/10 min
Density—ASTM D7921.2g/cm³
Heat deflection temperature0.46 MPaASTM D648118°C
Surface resistance—ASTM D25710¹⁵Ω·cm
Flammability1.5 mmUL 94 †V-2—
Injection molding conditions
Drying temperature110 °CDrying time4–5 h
Injection temperature255–275 °CMold temperature80 °C

Flammability V-2 at 1.5 mm; 912 kg/cm² flexural strength, 110% elongation and 13.8 g/10 min melt flow.