Aramid Reinforced POM Pellets DGK-POM FL100T

Aramid fiber POM composite for gears, bushings and wear-resistant moving parts

POM aramid fiber composite; wear-resistant, self-lubricating and dimensionally stable.

Aramid reinforced POM compound DGK-POM FL100T for gears, bushings, sliders, moving mechanisms, wear-resistant supports and molded parts requiring strength, durability and stable friction performance. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
POM
Model
DGK-POM FL100T
Color
Custom color matching supported
Processing
Injection molding. Injection molding, extrusion or other processes according to the formula.
Key performance
POM aramid fiber composite; wear-resistant, self-lubricating and dimensionally stable.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can wear resistance and friction be customized?

Yes. PTFE, MoS2, aramid or other wear additives can be adjusted according to the mating material, load and movement speed.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-POM FL100T or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1chair castors
Application area 2gears
Application area 3guide sliders
Application area 4bushings
Application area 5rollers
Application area 6textile machine sliding parts

Reference quote

Minimum price
USD 5.9/kg
Maximum price
USD 10.8/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePOM aramid fiber compositeSpecificationDGK-POM FL100T
Material propertiesWear-resistant, self-lubricating, dimensionally stableColorNatural color
UseGears, bushings, sliders, guide blocks, precision wear partsSample statePellets
Processing methodInjection molding-/
ItemConditionMethodDataUnit
Mechanical Properties
Bending strength/Typical range60-116MPa
Flexural modulus/Typical range2000-4070MPa
Tensile strength/Typical range40-82.7MPa
Tensile modulus/Typical average~3300MPa
Elongation at break/Typical range2-12%
Izod notched impact strength/ISO typical range5-8kJ/m2
Izod unnotched impact strength/ISO typical range32-45kJ/m2
Others
Density/Typical range1.37-1.52g/cm3
Heat distortion temperature1.8 MPaTypical range87-154℃
Friction coefficientDry frictionGB/T 3960 ref.0.15-0.20/
Wear amount200 N, 0.42 m/s, 120 minGB/T 3960-2016 ref.13mg
Surface resistivity/Typical range10^4-10^9ohm/sq
FlammabilityUL-94TypicalHB/
Injection molding process
Drying temperature80℃Drying time/
Injection temperature195-210℃Mold temperature90-100℃

Contact