Wear-Resistant POM with MoS₂ DGK-POM M90G
MoS₂-lubricated POM for gears, pumps and guide rails
DGK-POM M90G is a wear-resistant POM compound with molybdenum disulfide (MoS₂) and glass fiber reinforcement, supplied as gray pellets for injection molding and extrusion. A 128 °C heat deflection temperature at 1.8 MPa and 1.64 g/cm³ density give gears, pump components and guide rails a dense, stiff structure for loaded drive duty.
Gears in drive assemblies, pump components and guide rails for sliding assemblies are the target parts. Heat deflection temperature reaches 170 °C at 0.5 MPa (ASTM D648), melting point is 185 °C, and mold shrinkage of 1.9–2.2% suits dimensionally stable gear teeth and rail profiles in both injection molding and extrusion.
Important parameters
- Base resin
- POM
- Model
- DGK-POM M90G
- Color
- Gray
- Processing
- Injection molding and extrusion
- Key performance
- Wear-resistant POM compound with molybdenum disulfide (MoS₂) and glass fiber reinforcement.
- Status
- Pellets
FAQ
What is this grade made of?
It is a wear-resistant POM compound combining molybdenum disulfide (MoS₂) lubrication with glass fiber reinforcement, supplied as gray pellets. Density is 1.64 g/cm³ and heat deflection temperature 128 °C at 1.8 MPa (ASTM D648), so gears and guide rails stay stiff under load.
What parts can use this grade?
Gray pellets suit gears in drive assemblies, pump components and guide rails for sliding assemblies. Heat deflection temperature is 170 °C at 0.5 MPa and mold shrinkage 1.9–2.2%, with a coefficient of linear thermal expansion of 10.4 ×10⁻⁵ m/(m·°C) from −40 to 29 °C for stable gear and rail dimensions.
How is it processed?
It runs in both injection molding and extrusion, supplied as pellets. Melting point is 185 °C (ASTM D2133), heat deflection temperature 128 °C at 1.8 MPa and density 1.64 g/cm³; the two processing routes cover molded gears and extruded guide rail profiles from the same grade.
How can I request a trial sample?
Share the part drawing, mating material, load and sliding speed and DEYU will match a DGK-POM M90G sample for a molding trial. Include the production route, injection molding or extrusion, and the target wall section, since mold shrinkage of 1.9–2.2% sets the tool allowance.
Application areas
| Application area | Typical parts |
|---|---|
| Drive assemblies | Gears |
| Pumps | Pump components |
| Sliding assemblies | Guide rails |
Reference quote
- Minimum price
- USD 4.80/kg
- Maximum price
- USD 5.20/kg
Final pricing is set by color, order quantity and project requirements.
Data sheet
Physical Property Data Sheet
| Name | POM/MoS₂ | Grade | DGK-POM M90G |
|---|---|---|---|
| Material properties | Wear-resistant POM compound with molybdenum disulfide (MoS₂) and glass fiber reinforcement. | Color | Gray |
| Specimen dimensions | 80 × 10 × 4 mm | Sample form | Pellets |
| Processing method | Injection molding and extrusion | — | — |
| Property | Condition | Test method | Value | Unit |
|---|---|---|---|---|
| Thermal properties | ||||
| Coefficient of linear thermal expansion | −40–29 °C | ASTM D696 | 10.4 | 10⁻⁵ m/(m·°C) |
| Coefficient of linear thermal expansion | 60–104 °C | ASTM D696 | 12.2 | 10⁻⁵ m/(m·°C) |
| Heat deflection temperature | 1.8 MPa | ASTM D648 | 128 | °C |
| Heat deflection temperature | 0.5 MPa | ASTM D648 | 170 | °C |
| Melting point | — | ASTM D2133 † | 185 | °C |
| Other properties | ||||
| Density | 23 °C | ASTM D792 | 1.64 | g/cm³ |
| Mold shrinkage | — | — | 1.9–2.2 | % |
| Flammability | — | UL 94 | HB | — |
Melting point 185 °C follows ASTM D2133; the sheet does not quantify glass fiber content.
The melting point and the reference ASTM D2133 (†) are transcribed from the original sheet; the test method requires confirmation. The glass fiber content is not specified.
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1