Flame-Retardant Conductive PP Pellets DGK-PP DD4-5A-JC
V-0 conductive PP with 10^3-10^5 ohm/sq resistance for electrical and ESD parts
V-0 flame retardant; conductive 10^3-10^5 ohm/sq; black.
Flame-retardant conductive PP compound DGK-PP DD4-5A-JC with V-0 rating and 10^3-10^5 ohm/sq resistance for conductive sheets, electrical structural parts, ESD housings, flame-retardant components and molded products. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- PP
- Model
- DGK-PP DD4-5A-JC
- Color
- Custom color matching supported
- Processing
- Extrusion / injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- V-0 flame retardant; conductive 10^3-10^5 ohm/sq; black.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can the resistance or ESD level be customized?
Yes. Resistance range, stiffness and processing balance can be adjusted according to wall thickness, part design and grounding requirements.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-PP DD4-5A-JC or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | ESD trays |
| Application area 2 | sensor housings |
| Application area 3 | medical device accessories |
| Application area 4 | conductive textile parts |
| Application area 5 | shielding covers |
| Application area 6 | low-resistance molded clips |
Reference quote
- Minimum price
- USD 4.1/kg
- Maximum price
- USD 10.3/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | PP composite | Specification | DGK-PP DD4-5A-JC |
|---|---|---|---|
| Material properties | Flame-retardant conductive PP | Color | Black |
| Use | Conductive sheets, electrical structural parts, ESD housings, flame-retardant molded components | Sample state | Pellets |
| Processing method | Injection molding / extrusion | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | / | GB/T 9341-2008 | 22 | MPa |
| Flexural modulus | / | GB/T 9341-2008 | 1023 | MPa |
| Tensile strength | 20 mm/min | GB/T 1040-2006 | 21.8 | MPa |
| Yield strength | / | GB/T 1040-2006 | 22 | MPa |
| Elongation at break | / | GB/T 1040-2006 | 90 | % |
| Charpy notched impact strength | / | GB/T 1043.1-2008 | 29 | kJ/m2 |
| Charpy unnotched impact strength | / | GB/T 1043.1-2008 | No fracture | kJ/m2 |
| Izod notched impact strength | / | GB/T 1843-2000 | 35 | kJ/m2 |
| Others | ||||
| Melt Flow Index | / | GB/T 3682-2000 | 7 | g/10 min |
| Density | / | GB/T 1033-1986 | 0.965 | g/cm3 |
| Heat distortion temperature | Method A, 120℃ | GB/T 1633-2000 | 105 | ℃ |
| Surface resistivity | / | GB/T 1401-2002 | 10^3-10^5 | ohm/sq |
| Flammability | UL-94 | GB/T 2408-1996 | V-0 | / |
| Injection molding process | ||||
| Drying temperature | 90℃ | Drying time | 4-5 h | |
| Injection temperature | 210-225℃ | Mold temperature | 80℃ | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1