UV-Resistant PP DGK-PP F130UV
Weather-resistant PP for appliance covers and sunlit housings
DGK-PP F130UV is a natural-color polypropylene built for UV exposure, weathering and aging resistance. A 4.8 g/10 min melt flow rate fills thin appliance covers and trim, while 25.98 MPa flexural strength and 0.95 g/cm³ density keep housings stiff and light.
Appliance covers, housings and control panel trim, plus protective covers for equipment installed in sunlight, are the main applications. The compound keeps 1126.46 MPa flexural modulus and 15% elongation at break, so snap fits and thin walls have room to flex, and the 112 °C Vicat softening temperature (GB/T 1633-2000) covers normal appliance service heat.
Important parameters
- Base resin
- PP
- Model
- DGK-PP F130UV
- Color
- Natural
- Processing
- Injection molding
- Key performance
- Natural-color PP pellets with a melt flow rate of 4.8 g/10 min and flexural strength of 25.98 MPa.
- Status
- Pellets
FAQ
What is this grade designed for?
It is a UV-resistant, weather-resistant PP grade for injection-molded appliance parts. The formulation targets resistance to UV exposure, weathering and aging, which suits covers, housings and trim used in sunlit positions. Mechanical data include 25.98 MPa flexural strength, 24.6 MPa tensile strength and 15% elongation at break.
What color and form are supplied?
Natural-color pellets, as listed on the data sheet. Density is 0.95 g/cm³ and melt flow rate 4.8 g/10 min, running with 85 °C drying for 4–5 hours, 195–210 °C injection temperature and a 70 °C mold. Flammability is UL 94 HB and flexural modulus 1126.46 MPa.
Does the data sheet specify an outdoor service life?
The sheet specifies UV, weathering and aging resistance without a numbered outdoor service life, so exposure duration is set through an outdoor trial of molded parts. The documented baseline is 25.98 MPa flexural strength, 1126.46 MPa flexural modulus and 15% elongation at break, which supports comparison between candidate grades before the trial.
Can I request a trial sample?
Send the part drawing, exposure conditions and molding requirements and DEYU will match a DGK-PP F130UV sample for your trial. Include wall thickness and any color target, since natural pellets can be molded as supplied or matched. Data to compare against are 25.98 MPa flexural strength and 8 kJ/m² Charpy notched impact strength to GB/T 1043.1-2008.
Application areas
| Application area | Typical parts |
|---|---|
| Appliances | Covers, housings and control panel trim |
| Sunlit installations | Housings and protective covers for equipment |
Reference quote
- Minimum price
- USD 3.00/kg
- Maximum price
- USD 3.20/kg
Final pricing depends on order quantity and project requirements.
Data sheet
Physical Property Data Sheet
| Name | PP | Grade | DGK-PP F130UV |
|---|---|---|---|
| Material properties | UV, weathering and aging resistance | Color | Natural |
| Application | Appliance parts | Sample form | Pellets |
| Processing method | Injection molding | — | — |
| Property | Condition | Test method | Value | Unit |
|---|---|---|---|---|
| Mechanical properties | ||||
| Flexural strength | — | GB/T 9341-2008 | 25.98 | MPa |
| Flexural modulus | — | GB/T 9341-2008 | 1126.46 | MPa |
| Tensile strength | 20 mm/min | GB/T 1040-2006 | 24.6 | MPa |
| Yield strength | — | GB/T 1040-2006 | 24.58 | MPa |
| Elongation at break | — | GB/T 1040-2006 | 15 | % |
| Charpy notched impact strength | — | GB/T 1043.1-2008 | 8 | kJ/m² |
| Izod notched impact strength | — | GB/T 1843-2000 | 8.6 | kJ/m² |
| Other properties | ||||
| Melt flow rate | — | GB/T 3682-2000 | 4.8 | g/10 min |
| Density | — | GB/T 1033-1986 | 0.95 | g/cm³ |
| Vicat softening temperature (see note) | A120 | GB/T 1633-2000 | 112 | °C |
| Flammability | UL-94 | GB/T 2408-1996 | HB | — |
| Injection molding conditions | ||||
| Drying temperature | 85 °C | Drying time | 4–5 h | |
| Injection temperature | 195–210 °C | Mold temperature | 70 °C | |
The 112 °C result is a Vicat softening temperature to GB/T 1633-2000, not a heat distortion value.
Typical values and molding settings are taken from the supplied data sheet. The original table calls the 112 °C result heat distortion temperature and cites GB/T 1633-2000, a Vicat softening test method.
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1