V-1 Flame-Retardant PP DGK-PP FR830H

V-1 flame-retardant PP for electrical and electronic parts

DGK-PP FR830H is a V-1 flame-retardant PP for electrical and electronic components, supplied in black or beige made to order. Flexural strength of 30 MPa, 110% elongation at break and 48.5 kJ/m² Charpy unnotched impact strength give covers and internal parts toughness, with 1.05 g/cm³ density keeping weight low.

Electronic housings, electrical equipment covers and internal parts, plus injection-molded appliance components, are the typical applications. A 110 °C Vicat softening temperature (GB/T 1633-2000) and 1314 MPa flexural modulus suit indoor electrical duty, and the 8 g/10 min melt flow rate fills thin covers and internal supports.

Important parameters

Base resin
PP
Model
DGK-PP FR830H
Color
Black or beige, made to order
Processing
Injection molding
Key performance
V-1. Molten material drips during burning.
Status
Pellets

FAQ

Does FR830H drip when it burns?

Yes, molten material drips during burning, and that behavior accompanies the V-1 classification on the data sheet. V-1 is a vertical burning rating above HB, so the grade suits electrical and electronic parts that need a self-extinguishing vertical burn result at 1.05 g/cm³ density.

Which colors are available?

Black and beige can be made to order. Both are produced against your order, so the color target is set when the sample is prepared; the physical property data and molding settings come from the beige-sample report. Injection temperature runs 185–205 °C with 90 °C drying for 3–4 hours and a 60 °C mold.

What does the property table cover?

The property table covers 80 × 10 × 4 mm specimens from the beige sample: 30 MPa flexural strength, 1314 MPa flexural modulus, 24 MPa tensile strength, 110% elongation at break and 6.3 kJ/m² Charpy notched impact strength. Molding settings are 185–205 °C injection with a 60 °C mold, and flammability is V-1 with molten drip.

How do I request a sample?

Share the part drawing, target wall thickness and color when requesting a sample, and DEYU will match a DGK-PP FR830H lot for trial molding. The beige-sample data give the starting point: 30 MPa flexural strength and an 8 g/10 min melt flow rate, with black or beige produced to order.

Application areas

Application areaTypical parts
ElectronicsElectronic housings
Electrical equipmentCovers and internal parts
AppliancesInjection-molded components

Reference quote

Minimum price
USD 2.60/kg
Maximum price
USD 3.00/kg

Final pricing depends on color, order quantity and project requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePPGradeDGK-PP FR830H
Material propertiesV-1. Molten material drips during burning.ColorBlack or beige, made to order
Specimen dimensions80 × 10 × 4 mmSample formPellets
Processing methodInjection molding——
PropertyConditionTest methodValueUnit
Mechanical properties
Flexural strength—GB/T 9341-200830MPa
Flexural modulus—GB/T 9341-20081314MPa
Tensile strength20 mm/minGB/T 1040-200624MPa
Yield strength—GB/T 1040-200624MPa
Elongation at break—GB/T 1040-2006110%
Charpy notched impact strength—GB/T 1043.1-20086.3kJ/m²
Charpy unnotched impact strength—GB/T 1043.1-200848.5kJ/m²
Izod notched impact strength—GB/T 1843-20007kJ/m²
Other properties
Melt flow rate—GB/T 3682-20008g/10 min
Density—GB/T 1033-19861.05g/cm³
Vicat softening temperature (see note)A120GB/T 1633-2000110°C
FlammabilityUL 94GB/T 2408-1996V-1. Molten material drips during burning.—
Injection molding conditions
Drying temperature90 °CDrying time3–4 h
Injection temperature185–205 °CMold temperature60 °C

Property values and molding settings come from the beige sample; the V-1 row lists no test thickness.

The physical property values and molding settings are from the beige-sample report. Its flammability row does not specify a test thickness. The 110 °C entry is labeled heat deflection temperature in the report, but GB/T 1633-2000 is a Vicat test method.