UV- and Heat-Resistant PP DGK-PP H1200UV

UV- and heat-resistant PP for outdoor covers and enclosures

DGK-PP H1200UV holds a 125 °C heat deflection temperature (GB/T 1634-2000) together with UV resistance and a 12 g/10 min melt flow rate. That combination suits outdoor equipment covers, protective housings and electronic accessory enclosures where sunlight and elevated temperature meet at 0.9 g/cm³ density.

Outdoor equipment covers, protective housings and enclosures for electronic assemblies are the intended parts. A 2300 MPa flexural modulus gives housings the stiffness they need, 40 MPa yield strength covers structural loading, and Rockwell 105 R hardness resists surface marking in handling; the 12 g/10 min melt flow rate fills thin enclosure walls.

Important parameters

Base resin
PP
Model
DGK-PP H1200UV
Color
Natural
Processing
Injection molding
Key performance
A UV-resistant grade with a heat deflection temperature of 125 °C and a melt flow rate of 12 g/10 min.
Status
Pellets

FAQ

What is this grade designed for?

It is a UV- and heat-resistant PP for injection molding, aimed at outdoor parts and electronic accessory housings. The grade pairs a 125 °C heat deflection temperature (GB/T 1634-2000) with 2300 MPa flexural modulus, 40 MPa yield strength and 12 g/10 min melt flow rate, so covers and enclosures keep their shape in sun and heat.

What does the 125 °C heat deflection temperature mean?

It is the heat deflection temperature on the data sheet, measured to GB/T 1634-2000. The figure marks the temperature at which a loaded specimen deflects, making it a short-term stiffness indicator for comparing grades. The sheet lists the value without a test load, so continuous service temperature follows from the load and wall thickness of your design.

What color and form are supplied?

Natural-color pellets at 0.9 g/cm³ density, supplied for injection molding. Reference settings are 90 °C drying for 4–5 hours, 210–225 °C injection temperature and an 80 °C mold. Rockwell hardness is 105 R, flexural modulus 2300 MPa and flammability UL 94 HB.

Can I request a trial sample?

Provide the part drawing, service temperature, UV exposure and molding requirements and DEYU will match a DGK-PP H1200UV sample for trial molding. Include the expected wall thickness and any continuous temperature target, so the specification lines up with the 125 °C heat deflection temperature and 2300 MPa flexural modulus.

Application areas

Application areaTypical parts
Outdoor productsEquipment covers and protective housings
Electronic accessoriesEnclosures and covers for electronic assemblies

Reference quote

Minimum price
USD 3.20/kg
Maximum price
USD 3.50/kg

Final pricing depends on order quantity and project requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePPGradeDGK-PP H1200UV
Material propertiesUV and heat resistanceColorNatural
ApplicationOutdoor products and electronic accessory housingsSample formPellets
Processing methodInjection molding——
PropertyConditionTest methodValueUnit
Mechanical properties
Flexural modulus—GB/T 9341-20082300MPa
Yield strength—ISO 8256:2004 †40MPa
Unnotched cantilever impact strength23 °CGB/T 1843-2000 †25.6J/m
Other properties
Melt flow rate—GB/T 3682-200012g/10 min
Density—GB/T 1033-19860.9g/cm³
Heat deflection temperature—GB/T 1634-2000 †125°C
Rockwell hardness—GB/T 9341-1988 †105R
FlammabilityUL-94GB/T 2408-1996HB—
Injection molding conditions
Drying temperature90 °CDrying time4–5 h
Injection temperature210–225 °CMold temperature80 °C

Heat deflection temperature 125 °C to GB/T 1634-2000; flexural modulus 2300 MPa and melt flow 12 g/10 min.

Contact

Focused on modified plastic R&D and production

We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.