Flame-Retardant UV-Resistant PP DGK-PP J130UV

Impact-tough, UV-resistant PP for outdoor housings and grilles

DGK-PP J130UV combines UV resistance, impact toughness and stiffness for outdoor equipment and appliance housings. Charpy notched impact strength reaches 5.5 kJ/m² with no break in the unnotched test, flammability is UL 94 HB, and the 120 °C heat deflection temperature at 1.82 MPa holds shape in hot enclosures.

Outdoor communications equipment housings, air conditioner covers and molded ventilation grilles are the target parts. A 53 MPa flexural strength and 28.2 MPa tensile strength give the housings structural capacity, 24.3% elongation at break absorbs impact, and 1.1% molding shrinkage keeps grille openings and cover fits within tolerance.

Important parameters

Base resin
PP
Model
DGK-PP J130UV
Color
Transparent (per data sheet)
Processing
Injection molding
Key performance
Charpy notched impact strength of 5.5 kJ/m². No break in the unnotched test. Flammability rating: UL 94 HB.
Status
Pellets

FAQ

Which parts is this PP intended for?

It is an injection molding grade for outdoor communications equipment housings, air conditioner covers and appliance components. UV resistance handles sunlight, 5.5 kJ/m² Charpy notched impact strength handles knocks, and 53 MPa flexural strength with 28.2 MPa tensile strength gives the structural base at 1.2 g/cm³ density.

What is the UL 94 rating?

The data sheet lists UL 94 HB, the horizontal burning classification. HB covers applications where a horizontal burning result is sufficient rather than a vertical burn rating. The rating sits alongside a 120 °C heat deflection temperature at 1.82 MPa, so the grade suits covers and grilles in warm outdoor equipment.

How does it perform in impact tests?

The notched Charpy result is 5.5 kJ/m² and the unnotched specimen did not break, both to GB 1043-93. That combination marks a grade that absorbs impact in covers and grilles, while 1.1% molding shrinkage keeps dimensions stable. Elongation at break is 24.3% and flexural strength 53 MPa.

How can I request a trial sample?

Share the part drawing, wall thickness, UV exposure and target performance and DEYU will match a DGK-PP J130UV sample for trial molding. Include color and finish direction, since the data sheet lists a transparent color. A molded trial part is the clearest view of final appearance at your wall section.

Application areas

Application areaTypical parts
Outdoor equipmentCommunications equipment housings and protective covers
AppliancesAir conditioner covers and ventilation grilles

Reference quote

Minimum price
USD 3.10/kg
Maximum price
USD 3.30/kg

Final pricing depends on order quantity and project requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePPGradeDGK-PP J130UV
Material propertiesUV resistance, high impact strength and UL 94 HBColorTransparent (per data sheet)
ApplicationOutdoor equipment and appliance partsSample formPellets
Processing methodInjection molding——
PropertyConditionTest methodValueUnit
Physical properties
Density—GB 1033-961.2g/cm³
Mechanical properties
Molding shrinkage——1.1%
Elongation at break—GB 1040-9224.3%
Tensile strength—GB 1040-9228.2MPa
Flexural strength—GB 9341-8853MPa
Charpy notched impact strength—GB 1043-935.5kJ/m²
Charpy unnotched impact strength—GB 1043-93No breakkJ/m²
Thermal and flammability properties
Heat deflection temperature1.82 MPaGB 1634-88120°C
Flammability—UL 94HB—

HB is the horizontal burning classification; heat deflection 120 °C is measured at 1.82 MPa.

Values are typical results from the supplied data sheet. HB is a horizontal burning classification. Confirm flammability and weathering requirements at the intended part thickness and exposure conditions.

Contact

Focused on modified plastic R&D and production

We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.