Wear-Resistant PPO/PA Alloy Pellets DGK-PPO/PA U35
Self-lubricating PPO/PA alloy for sliding parts and wear-resistant mechanisms
PPO/PA alloy with strong wear resistance and self-lubricating behavior for sliding and friction parts.
Wear-resistant self-lubricating PPO/PA alloy compound DGK-PPO/PA U35 for sliding parts, wear components, moving mechanisms, guide elements, mechanical supports and molded parts needing stable friction behavior. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- PPO/PA
- Model
- DGK-PPO/PA U35
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- PPO/PA alloy with strong wear resistance and self-lubricating behavior for sliding and friction parts.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can wear resistance and friction be customized?
Yes. PTFE, MoS2, aramid or other wear additives can be adjusted according to the mating material, load and movement speed.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-PPO/PA U35 or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | chair castors |
| Application area 2 | gears |
| Application area 3 | guide sliders |
| Application area 4 | bushings |
| Application area 5 | rollers |
| Application area 6 | textile machine sliding parts |
Reference quote
- Minimum price
- USD 5.9/kg
- Maximum price
- USD 10.8/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Technical data
Engineering Data Availability Table
| Name | Wear-Resistant PPO/PA Alloy Pellets DGK-PPO/PA U35 | Specification | DGK-PPO/PA U35 |
|---|---|---|---|
| Material properties | PPO/PA alloy with strong wear resistance and self-lubricating behavior for sliding and friction parts. | Color | Custom color matching supported |
| Sample state | Pellet compound | Processing method | Injection molding. Injection molding, extrusion or other processes according to the formula. |
| Data status | Engineering confirmation required | - | Contact a DEYU engineer |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Wear Properties | ||||
| Wear amount | / | / | Contact a DEYU engineer | / |
| Friction coefficient | / | / | Contact a DEYU engineer | / |
| Self-lubricating performance | / | / | Contact a DEYU engineer | / |
| Basic Properties | ||||
| Melt Flow Index | / | / | Contact a DEYU engineer | / |
| Density | / | / | Contact a DEYU engineer | / |
| Mechanical Properties | ||||
| Tensile strength | / | / | Contact a DEYU engineer | / |
| Bending strength | / | / | Contact a DEYU engineer | / |
| Flexural modulus | / | / | Contact a DEYU engineer | / |
| Izod notched impact strength | / | / | Contact a DEYU engineer | / |
| Thermal Properties | ||||
| Heat distortion temperature | / | / | Contact a DEYU engineer | / |
| Vicat softening point | / | / | Contact a DEYU engineer | / |
| Processing Recommendations | ||||
| Drying temperature | Contact a DEYU engineer | Drying time | Contact a DEYU engineer | |
| Injection temperature | Contact a DEYU engineer | Mold temperature | Contact a DEYU engineer | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1