Permanent Antistatic PVC Pellets DGK-PVC KJD789JC
White permanent antistatic PVC with 10^6-10^9 ohm/sq resistance for extrusion
White permanent antistatic PVC; surface resistivity 10^6-10^9 ohm/sq; colorable formula and adjustable hardness up to 120 degrees.
Permanent antistatic PVC compound DGK-PVC KJD789JC with 10^6-10^9 ohm/sq resistance for extruded profiles, pipes, sheets, ESD covers, industrial parts and PVC products requiring stable static dissipation. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- PVC
- Model
- DGK-PVC KJD789JC
- Color
- Custom color matching supported
- Processing
- Extrusion / injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- White permanent antistatic PVC; surface resistivity 10^6-10^9 ohm/sq; colorable formula and adjustable hardness up to 120 degrees.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can the resistance or ESD level be customized?
Yes. Resistance range, stiffness and processing balance can be adjusted according to wall thickness, part design and grounding requirements.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-PVC KJD789JC or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | ESD trays |
| Application area 2 | sensor housings |
| Application area 3 | medical device accessories |
| Application area 4 | conductive textile parts |
| Application area 5 | shielding covers |
| Application area 6 | low-resistance molded clips |
Reference quote
- Minimum price
- USD 4.1/kg
- Maximum price
- USD 10.3/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Technical data
Engineering Data Availability Table
| Name | Permanent Antistatic PVC Pellets DGK-PVC KJD789JC | Specification | DGK-PVC KJD789JC |
|---|---|---|---|
| Material properties | White permanent antistatic PVC; surface resistivity 10^6-10^9 ohm/sq; colorable formula and adjustable hardness up to 120 degrees. | Color | Custom color matching supported |
| Sample state | Pellet compound | Processing method | Extrusion / injection molding. Injection molding, extrusion or other processes according to the formula. |
| Data status | Engineering confirmation required | - | Contact a DEYU engineer |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Electrical Properties | ||||
| Surface resistivity | / | / | Contact a DEYU engineer | / |
| Antistatic durability | / | / | Contact a DEYU engineer | / |
| Basic Properties | ||||
| Hardness | / | / | Contact a DEYU engineer | / |
| Density | / | / | Contact a DEYU engineer | / |
| Melt Flow Index | / | / | Contact a DEYU engineer | / |
| Mechanical Properties | ||||
| Tensile strength | / | / | Contact a DEYU engineer | / |
| Elongation at break | / | / | Contact a DEYU engineer | / |
| Tear strength | / | / | Contact a DEYU engineer | / |
| Thermal Properties | ||||
| Heat aging resistance | / | / | Contact a DEYU engineer | / |
| Flammability | / | / | Contact a DEYU engineer | / |
| Processing Recommendations | ||||
| Drying temperature | Contact a DEYU engineer | Drying time | Contact a DEYU engineer | |
| Processing temperature | Contact a DEYU engineer | Mold temperature | Contact a DEYU engineer | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1